Solution process parameters optimized for electrospinning of nanofibrous mats.

Solution Parameters
Polymer concentrations 10, 12, 14 %w/v
Starch: PVOH 30:70 w/w
Solvent System 10% Ethanol
Electrospinning process Parameters
Applied voltage 25 kV
Spinning Distance 13 cm