Effect of nano-silver hydrogel coating film on rabbit scalded model.

Group n The burn area of different time after treatment and the weight difference of the former paper (mg)
Day 6 Day 12 Day 18
Blank group 6 0 ± 0** 0 ± 0** 0 ± 0**
Model group 6 31.90 ± 27.13 82.05 ± 29.71 137.52 ± 26.03
Jingwanhonggroup 6 69.68 ± 33.56* 124.55 ± 35.16* 164.62 ± 35.38
High dose of nano-silver hydrogel coating film group 6 63.55 ± 25.67* 108.92 ± 30.45 147.97 ± 13.90
Medium dose of nano-silver hydrogel coating film group 6 69.08 ± 37.21 118.33 ± 18.16* 166.50 ± 20.46*
Low dose of nano-silver hydrogel coating film group 6 68.52 ± 11.06* 107.17 ± 7.18 158.73 ± 18.69

Note: compared with the model control group.

**

P < 0.01.

*

P < 0.05.