Skip to main content
. 2017 Jul 19;50(15):5711–5718. doi: 10.1021/acs.macromol.7b00919

Table 1. Dry Thickness, Mn, PDI, and Grafting Density of PMMA Brushes Synthesized under Different Degrees of Confinement by SI-ATRP.

degree of confinement (d, μm) thickness (nm) Mn (kDa) PDI grafting density (chains nm–2)
0.4 196 ± 16 390 2.20 0.35
10 92 ± 10 200 1.59 0.31
30 49 ± 4 125 1.23 0.27
50 49 ± 3 122 1.12 0.28
open (∞) 48 ± 5 121 1.11 0.28