Skip to main content
. 2018 Mar 28;10(16):14175–14182. doi: 10.1021/acsami.8b02177

Figure 2.

Figure 2

Low-coverage regime of sexiphenyl on In2O3(111) after annealing at 200 °C; imaged with STM at 80 K. The unit cell of the In2O3 substrate is indicated in white. (a, b) Sub-monolayer coverages. (c) “Open monolayer”.