. 2018 Apr 2;9(17):4071–4082. doi: 10.1039/c8sc00762d

Fig. 2. (a) DLS particle size distributions recorded for 0.10% w/w dispersions of PBeMA37–PBzMAx diblock copolymer spheres in n-dodecane at 50 °C. (b) The apparent hydrodynamic diameter (D) determined by DLS at 50 °C vs. PBzMA DP (x) plot indicates an α scaling exponent of 2/3. (c) TEM images for selected PBeMA37–PBzMAx spheres obtained after drying 0.10% w/w dispersions in n-dodecane. See Fig. S3 for additional higher magnification TEM images.

Fig. 2