Skip to main content
. 2018 Apr 2;9(17):4071–4082. doi: 10.1039/c8sc00762d

Fig. 5. Temperature dependence of the storage modulus (G′, blue squares) and loss modulus (G′′, red circles) for a 20% w/w dispersion of 32 nm PBeMA37–PBzMA100 spherical nanoparticles in mineral oil on cooling from 50 °C to 20 °C (filled symbols) and on heating from 20 °C to 50 °C (open symbols). Data were recorded at 1.0% strain amplitude using an angular frequency of 10 rad s–1, with 5 min being allowed for thermal equilibration between each measurement.