Skip to main content
. 2018 Mar 23;18(4):958. doi: 10.3390/s18040958

Figure 3.

Figure 3

SEM surface and cross-sectional images of ITO and In2O3 films with 8 wt % glass additives annealed at 1250 °C with different measuring times. (A,C) ITO film; (B,D) In2O3 film.