Table 1.

Electrospinning parameters and frequency shift after coating with PAN nanofiber.

Trial Time (s) Frequency Shift (Hz) Deposited Mass (µg)
PAN-NF 1 10 150 0.2
PAN-NF 2 20 500 0.6
PAN-NF 3 30 900 1.0
PAN-NF 4 40 1500 1.7