(a) Photoluminescence images of small-pore pSi particles (∼2 mg) dispersed in a microtiter well containing 2 M KOH (200 μL), displayed as a time series. Excitation source was a 365 nm light-emitting diode and images were obtained using a NIR camera fitted with a 600 nm long-pass filter. The porous Si particles were prepared by 35 min oxidation at 700 °C, corresponding to the “medium oxide shell” material of Table 1. (b) Plot of photoluminescence intensity, integrated as a sum of pixel intensities (ImageJ), as a function of time.