Temperature rise (°C) recorded during the photopolymerisation process for the analysed materials, according to light source and curing mode. All the results are reported in terms of mean values and standard deviation (in brackets).

Light Source EPH DEI CLM SDR
Laser (Mode I) 19.2 (±1.7) 15.4 (±1.1) 14.4 (±1.3) 18.7 (±1.5)
Laser (Mode II) 14.5 (±0.9) 10.1 (±0.7) 9.8 (±0.8) 14.6 (±1.2)
LED Mectron (Mode I) 16.3 (±1.3) 12.2 (±1.3) 12.1 (±1.4) 15.3 (±1.5)
LED Enfis (Mode II) 15.2 (±1.5) 9.5 (±0.8) 10.4 (±1.3) 16.2 (±1.4)