Sample SBET (m2/g) Vpore (cm3/g) Vmic (cm3/g) Vmic/Vpore (%)
UiO-66 838 0.245 0.224 91
UiO-66-NH2 822 0.236 0.214 90
UiO-66/GO 1184 0.384 0.304 79
UiO-66-NH2/GO 1052 0.345 0.286 83

SBET is the BET surface area; Vpore is total pore volume; Vmic is micropore volume.