. 2018 Apr 16;11(4):608. doi: 10.3390/ma11040608

Figure 13.

Figure 13

SEM micrographs of shear fracture surfaces of (a) 1.0-GNFs; and (b) 1.5-GNFs nanocomposites sintered at 1000 °C, respectively.