Skip to main content
. 2018 Apr 24;30(9):2945–2953. doi: 10.1021/acs.chemmater.8b00321

Figure 3.

Figure 3

(a) Contact angle and QCM-D measurements of the copolymers in 0.1 M NaCl aqueous solutions and (b) thin film cyclic voltammetry measurements of P-0, P-50, and P-100 and a blank ITO electrode in degassed 0.1 M NaCl aqueous solution with a scan rate of 100 mV/s vs Ag/AgCl.