Skip to main content
. 2018 May 17;8:7758. doi: 10.1038/s41598-018-25948-x

Figure 1.

Figure 1

(a) PL spectra and cross-sectional SEM images of ZnO-C:NW and ZnO-NW. Inset shows the magnified view of PL range of 400–700 nm. (b) Room-temperature M-H curves of ZnO-C:NW and ZnO-NW. Upper and lower insets present magnetic field applied parallel to growth direction (c-axis) and magnified M-H loops of ZnO-C:NW and ZnO-NW, respectively, at 300 K.