(a) Normalized O K-edge and (b) Zn L3,2-edge XANES spectra with photon helicity of incident X-rays parallel (μ+) and anti-parallel (μ) to direction of magnetization for ZnO-C:NW and ZnO-NW. Upper inset in Fig. 4(a) displays magnified O K-edge XANES spectra; lower panels in Fig. 4(a,b) display O K-edge and Zn L3,2-edge XMCD spectra of ZnO-C:NW and ZnO-NW. (c) C K-edge XANES spectra of ZnO-C:NW. Upper inset magnified view C K-edge near-edge spectra of ZnO-C:NW. Lower panel displays C K-edge XMCD spectra of ZnO-C:NW.