Skip to main content
. 2018 May 15;6:159. doi: 10.3389/fchem.2018.00159

Figure 2.

Figure 2

(A) XRD patterns of 0.5Li2MnO3·0.5LiNi0.5Co0.2Mn0.3O2 synthesized at 900°C by using different lithium sources and magnified XRD patterns in the 2θ range of (B) 19°–23°, (C) 35°–39°, (D) 42°–47°, (E) 63°–67°, respectively.