Skip to main content
. 2015 Nov 10;7(2):1224–1232. doi: 10.1039/c5sc03419a

Fig. 5. The first CV scans at 0.1 mV s–1 and GCD curves at 160 mA g–1 of CF10–Spore, CF20–Spore, CF25–Spore, and CF30–Spore in TEGDME electrolyte (a) and (b) respectively, and in EC/DEC electrolyte (c) and (d), respectively.

Fig. 5