Skip to main content
. 2018 May 2;8(5):294. doi: 10.3390/nano8050294

Figure 2.

Figure 2

Transmission electron microscope (TEM) (a,c,e) and high-resolution transmission electron microscope (HRTEM) (b,d,f) images of the powders of the raw anatase TiO2 (a,b) and the samples 2Si (c,d) and 2Si-N (e,f) milled at the speed of 800 rpm.