Skip to main content
. 2018 May 15;11(5):801. doi: 10.3390/ma11050801

Figure 8.

Figure 8

Indentation hardness HIT across the 100Cr6 steel surface, tested in three different regions: polished (black triangles), fs-laser processed (LSFL-covered, blue squares), and across the center of an RSTT wear track (RSTT: normal force 1.0 N, stroke 1 mm, frequency 1 Hz, cycles 100,000, Castrol VP-1) in the fs-laser-processed (LSFL-covered, red circles) area.