Skip to main content
. 2018 May 17;11(5):829. doi: 10.3390/ma11050829

Figure 7.

Figure 7

Rietveld refinement for Al2O3–20 wt % ZrO2 after annealing at 600 °C for 2 h (a), 1200 °C (c), 1400 °C (e), and Al2O3–40 wt % of ZrO2 after annealing at 600 °C for 2 h (b), 1200 °C (d), 1400 °C (f).