Raman spectral data for Al2O3–(40,20 wt %) ZrO2 after annealing at 600 °C and 1400 °C [45,52,53,54,55].

Al2O3–(20,40 wt %) ZrO2 after Annealing at 600 °C Wavenumbers (cm−1) Literature Al2O3–(20,40 wt %) ZrO2 after Annealing at 1400 °C Wavenumbers (cm−1) Literature
Al2O3–(20 wt %) ZrO2 after annealing at 1400 °C
t-ZrO2 148, 265, 312 [49] t-ZrO2 147, 270, 315, 459 [49]
m-ZrO2 177, 188, 215, 355, 382, 477, 513, 559, 637 [49] m-ZrO2 179, 190, 381, 419, 578, 647 [49]
γ-Al2O3 234, 404 [52,53] α-Al2O3 381, 419, 431,578,647, 751 [52,53,54,55]
Al2O3–(40 wt %) ZrO2 after annealing at 1400 °C
t-ZrO2 145,269, 314, 456 [49]
m-ZrO2 179, 190, 336, 351, 380, 417, 477, 507, 598, 647 [49]
α-Al2O3 380, 417, 647, 753 [52,53,54,55]