Skip to main content
. 2018 May 17;11(5):831. doi: 10.3390/ma11050831

Figure 3.

Figure 3

Oxygen storage capacity of MgFexAl2−xO4 materials as a function of the Fe2O3 content. Note that when Fe2O3 loading is less than 30 wt %, it is completely incorporated into the spinel structure without separate Fe2O3 phases. Inline graphic: iron incorporated in spinel structure; Inline graphic: separate Fe2O3 phase. Obtained from [81].