. 2018 Mar 26;8:5216. doi: 10.1038/s41598-018-23577-y

Figure 1.

Figure 1

Microhardness (a) and compressive strength (b) of CPC composites. V125-E8 had the highest values at all L/P ratios; DW had the lowest. V125-E8 had a microhardness 2- to 7-fold higher and a compressive strength >10-fold higher than DW. The microhardness and compressive strength tended to decrease as the L/P ratio increased. However, the highest microhardness and compressive strength were observed at an L/P ratio of 0.4.