Skip to main content
. 2018 Jun 1;9:2152. doi: 10.1038/s41467-018-04394-3

Fig. 4.

Fig. 4

Impact of the Li-salt concentration on the Li density distribution. Li density at different stages of the first plating cycle and at the end of stripping at 1 mA cm−2 comparing 1 molar and 2 molar LiPF6 in EC/DMC. The depth is measured starting from the interface of the Cu current collector with the electrolyte/SEI/Li-metal