reference materials operating voltage (V) response time (s) recovery time (s) sensitivity (%)/ H2 (ppm)
this work oriented ZnO nanorods 6.0 60 49 33/2000
Wang et al. [11] ZnO nanorods 0.5 >300 <20 5/500
Hassan et al. [17] ZnO nanorods 400 187 0.4/20 000
Kadhim et al. [29] spin coat SnO2 0.2 192 95 2570/1000
Fields et al. [32] nanobelts SnO2 0.1 220 60/20 000
Xiang et al. [26] Pd/TiO2 nanotubes 120 90 8/10 000
Wang et al. [27] Nb2O5 nanowires 100 470 100/2000
Hassan et al. [33] ZnO nanorods 0.1 176 116 500/1000