Skip to main content
. 2018 Jun 7;8:8737. doi: 10.1038/s41598-018-27096-8

Figure 2.

Figure 2

X-ray diffraction (XRD) profiles, showing the graphite peak, obtained from as-mixed powder (zero hours milling) and powder sample milled for 80 h.