Skip to main content
. 2016 Jan 20;7(5):3188–3205. doi: 10.1039/c5sc04714e

Table 3. Results of the comparative OER studies on unprotected Ru nano-chain and Ru nanomaterials stabilized by TX-100, CTAB and SDS.

Catalyst E @ 10 mA cm–2 (mV) η @ 10 mA cm–2 (mV) Tafel (mV dec–1) Specific activity (mA cmECSA–2) TOF @ η = 308 mV (s–1)
Unprotected Ru0 nano-chain networks 1538 308 ± 2 95 0.1008 4.72
Ru0-TX-100 1673 443 163
Ru0-CTAB 1591 361 215
Ru0-SDS 1615 385 202