Figure 4.

Figure 4

Loss of (a) E. coli and (b) S. aureus viability after 1 h of UV exposure to planar TiO2-10, TiO2-50, and TiO2–C films. Control PET and NOA surfaces (no TiO2) are also shown. Two asterisks (**) denote 99% significance between control and TiO2-containing samples. Error bars denote standard error.