Skip to main content
. 2018 Jun 27;8:9764. doi: 10.1038/s41598-018-27949-2

Table 1.

Positron lifetimes with corresponding intensities for Fe, Co and FeCo.

Sample details τ1(ps) I1% τ2 (ps) I2% τ3 (ps) I3% τm (ps)
τ4 (ns) I4%
Fe powder 158 (4) 63 (3) 323 (18) 33 (2) 622 (55) 4 (1) 215
Co power 145 (6) 61 (6) 274 (26) 31 (4) 514 (27) 8 (2) 188
Fe rod 140 (1) 86 (1) 268 (6) 14 (1) 0 0 158
Co rod 156 (1) 95 (1) 283 (19) 5 (1) 0 0 162
FeCo as prepared 180 (10) 9.5 (1) 345 (1.1) 87.5 (1) 1852 (172) 0.5 (0.01) 329
54 (0.4) 2.5 (0.1)
FeCo annealed at 700 °C 133 (7) 38 (2.8) 284 (6.7) 59 (2) 698 (31) 3 (0.5) 225
FeCo annealed at 800 °C 133 (2.6) 59.5 (1.5) 292 (4.7) 39.6 (1) 959 (61) 0.9 (0.1) 197