Fig. 6. Dependence of the current density values of TiO2-AR electrode (a) and TiO2-R electrode (b) on the number of calcination cycles. After calcination treatment at 1073 K for 120 min (4 minutes per cycle and 30 cycles), the TiO2-AR was converted to pure rutile phase.