Skip to main content
. 2018 Jun 16;11(6):1028. doi: 10.3390/ma11061028

Figure 1.

Figure 1

Appearances of GFRP bars after elevated temperatures exposure: (a) at 100 °C and holding time of 2 h; (b) at 150 °C and holding time of 0 h; (c) at 200 °C and holding time of 2 h; (d) at 250 °C and holding time of 0 h; (e) at 300 °C and holding time of 1 h; (f) at 350 °C and holding time of 0 h.