Table 4.
Flame Retardant Composites | T10%/°C | T20%/°C | T50%/°C | W600/% |
---|---|---|---|---|
NR | 349 | 367 | 396 | 27 |
NR/IFR | 292 | 352 | 403 | 32 |
NR/IFR/MCM-41 | 289 | 356 | 403 | 35 |
NR/IFR/GO | 287 | 355 | 401 | 33 |
NR/IFR/GO-MCM-41 | 290 | 356 | 404 | 35 |
Flame Retardant Composites | T10%/°C | T20%/°C | T50%/°C | W600/% |
---|---|---|---|---|
NR | 349 | 367 | 396 | 27 |
NR/IFR | 292 | 352 | 403 | 32 |
NR/IFR/MCM-41 | 289 | 356 | 403 | 35 |
NR/IFR/GO | 287 | 355 | 401 | 33 |
NR/IFR/GO-MCM-41 | 290 | 356 | 404 | 35 |