Skip to main content
. 2018 Jun 20;11(6):1044. doi: 10.3390/ma11061044

Figure 8.

Figure 8

OM images of the samples deformed at 1200 °C with the strain rate of (a) 1 s−1; (b) 0.1 s−1; (c) 0.01 s−1; (d) 0.001 s−1.