Skip to main content
. 2018 Jun 18;11(6):1031. doi: 10.3390/ma11061031

Figure 1.

Figure 1

Scanning electron microscopy images presenting the morphologies of used fillers: glass fillers with a mean particle size of 0.7 μm (a); 2 μm (b); silica nanofiller (c); and silver sodium hydrogen zirconium phosphate (d,e).