. 2018 Jun 13;8(6):429. doi: 10.3390/nano8060429

Figure 3.

Figure 3

XRD pattern of CuNPs/NGO (carbonized at 600 °C (a), 700 °C (b), 800 °C (c) and 900 °C (d)).