. 2018 Mar 15;122(25):13682–13690. doi: 10.1021/acs.jpcc.8b00145

Figure 1.

Figure 1

(A) Comparison of the UV–vis spectrum, recorded for a PEDOT layer (Qpol = 25 mC cm–2), at E = −0.9 V in 0.1 M Na2SO4 solution, saturated with Ar with the irradiance spectrum of the solar simulator. (B) Photovoltammogram recorded in 0.1 M Na2SO4 saturated with Ar for a PEDOT film, electrodeposited with optimal polymerization charge density (Qpol = 50 mC cm–2) on glassy carbon electrode. The sweep rate was kept at 2 mV s–1, while the light-chopping frequency was 0.1 Hz. (C) Maximum photocurrent vs polymerization charge density plot.