Skip to main content
. 2018 Mar 15;122(25):13682–13690. doi: 10.1021/acs.jpcc.8b00145

Figure 2.

Figure 2

(A) SEM images of a bare CNT layer on GC (mCNT = 60 μg cm–2), (B, C) PEDOT/CNT nanocomposite layer on GC (mCNT = 60 μg cm–2), Qpol = 400 mC cm–2, (D) graphene layer on GC (mgraphene = 110 μg cm–2), and (E, F) PEDOT/graphene layer on GC (mgraphene = 110 μg cm–2), Qpol = 200 mC cm–2.