Figure 4.

Figure 4

Raman spectra of (A) CNT (black line), PEDOT (blue line), and PEDOT/CNT (red line) samples (mCNT = 60 μg cm–2, Qpol= 400 mC cm–2) and (B) graphene (black line), PEDOT (blue line), and PEDOT/graphene (red line) samples (mgraphene = 110 μg cm–2, Qpol = 200 mC cm–2).