Table 5.

Fraction of Br-CuIIL+ Bound to SDS Interfaces in Micellar Systems or in Miniemulsions, T = 65 °C.

catalyst environment fbound
Br-CuIITPMA+ micellesa 0.79
Br-CuIITPMA+ miniemulsionb 0.95
Br-CuIIMe6TREN+ miniemulsionb <0.50
Br-CuIIBPMEA+ miniemulsionb 0.64
a

Water + 0.1 M NaBr + 10−3 M CuIIBr2/TPMA + 0.028 M SDS.

b

Cn-BuA/CNaBr/CCuIIBr2/CL= 280/20/0.2/0.4, 20% v/v BA in water, SDS = 28 mM = 4.6 wt % relative to BA, HD = 10.8 wt % relative to BA.