Skip to main content
. Author manuscript; available in PMC: 2019 Aug 10.
Published in final edited form as: J Control Release. 2018 May 22;283:84–93. doi: 10.1016/j.jconrel.2018.05.025

Fig. 1.

Fig. 1

(A) Representative TEM image of rNG-DFO (scale: 500 nm). (B) Under oxidative stimuli, thioketals in the nanogels cleave and acetone is released as nanogels degrade into water-soluble polymeric fragments. Shown below are degradation profiles as monitored by DLS for rNG-DFO incubated with 100 μM H2O2 at 0 h (black line), 12 h (red line) and 24 h (blue line). (C) Representative UV-Vis absorption spectrum of DFO, rNG and rNG-DFO in the absence and presence of iron(III) reveal that only DFO and rNG-DFO display the characteristic absorbance peak at 430 nm for the DFO:iron(III) complex.