Skip to main content
. 2018 Jul 4;4(7):e00680. doi: 10.1016/j.heliyon.2018.e00680

Fig. 5.

Fig. 5

A) Sugar glass construct (loaded with CaCl2 with two supporting branches. B) Sugar glass construct (loaded with CaCl2) without the supporting branches. C) Sugar glass construct (loaded with CaCl2) filled with ALG. D) Remaining ALG gel after 10 minutes of gelation and 100 seconds of sugar dissolution in an ultrasound bath. E) Remaining alginate gel after approximately 18 hours in a demineralized water bath. F) Alginate gel immediately after the perfusion with red-dyed water. Scale bar 10 mm.