Skip to main content
. 2018 Jun 25;51(13):4813–4820. doi: 10.1021/acs.macromol.8b00892

Figure 8.

Figure 8

Main effects on viscoelastic behavior of hydrogels caused by SDS and urea. (a) Relaxation time derived from data in Figure 6; (b) plateau modulus, taken at ω = 100 rad/s, plotted as a function of SDS/urea concentration.