Table 1. Gaussian Fitting XPS Results of Osite3 for Catalyst Samples.
fitting parameter | ZnAl2O4–H | ZnAl2O4–S | ZnAl2O4–C |
---|---|---|---|
B.E (eV) | 532.37 | 532.43 | 532.5 |
area | 530 | 332 | 310 |
rel. content (%) | 11.57 | 8.60 | 8.18 |