Figure 1

(a) Scheme for the synthesis and surface functionalization of ZGO, (b) transmission electron micrograph (TEM) images of ZGO, (c) excitation (em 700 nm) and emission (ex 254 nm) spectra of ZGO, and (d,e) NIR persistent luminescence decay curve of ZGO at 700 nm after 5 min of irradiation with a 254 nm UV lamp and 655 nm LED; insets: the afterglow emission spectra after irradiation with a 254 nm UV lamp and 655 nm LED.