Skip to main content
. 2017 Dec 26;10:49–67. doi: 10.1016/j.jare.2017.12.004

Fig. 7.

Fig. 7

(a) Schematic depicting precipitate-free zones (PFZ) at grain boundary and accumulation of a stress concentration on Grain boundary triple junction (GBTJ) [66]; (b) SEM depicting intergranular fracture and a population of micro-voids along to the grain boundary crack for AA 8090 Al-Li alloy [66].