Skip to main content
. 2018 Jul 15;18(7):2289. doi: 10.3390/s18072289

Figure 7.

Figure 7

Comparison between the experimental distributions of the breakdown voltages of the detectors with 10 µm epitaxy and the simulations. A good agreement is observed for all the edge structures with the exception of the detectors without edge structure and the detectors with 16 epi rings.