Skip to main content
. 2018 Jul 21;8(7):556. doi: 10.3390/nano8070556

Figure 3.

Figure 3

Scanning electron microscopy (SEM) images of the samples via pyrolysis of waste polyethylene with 0.75 wt% Ni catalyst at 773 K (a); 873 K (b); 973K (c); and 1073 K (d); and EDS of the nanoparticles in the area marked by the circles in Figure 3c in (e).