Skip to main content
. 2018 Jul 21;8(7):556. doi: 10.3390/nano8070556

Figure 5.

Figure 5

Scanning electron microscopy (SEM) images of final product samples resulting from pyrolysis of waste polyethylene at 973 K when adding different amounts of Ni catalysts: 0.25 wt% (a); 0.50 wt% (b); 0.75 wt% (c); and 1.00 wt% (d).