Table 3.

Compressive strength of pseudo-cements made from 45% acetic acid with ionomer glass (powder:liquid ratio 4:1) (Standard deviations in parentheses).

Storage time Compressive strength/MPa
1 day 11.9 (3.3)
1 week 24.8 (14.3)
1 month 72.0 (27.7)
3 months 104.4 (25.2)
6 months 104.5 (25.3)