. 2018 Jun 29;11(7):1109. doi: 10.3390/ma11071109

Figure 7.

Figure 7

Percentage change, over eight days, in the resistance of (a) 50 µm; and (b) 100 µm, wide Cu track exposed to saline through a protective layer of 5 µm of Parylene-C.